A Review Casting Defect Reduction in Manufacturing Industry Using Six Sigma

Author : Scholar Akshay Arzare, Professor Yogesh Ladhe Journa Name: INTERNATIONAL JOURNAL OF SCIENTIFIC RESEARCH AND ENGINEERING TRENDS Country : India Volume: 10 issue: 3 Year: 2024 Views : 458
Abstract:
The art of meeting customer specifications, which today is termed as “quality”. Quality is the symbol of human civilization, and with the progress of human civilization, quality control will play an incomparable role in the business. It can be said that if there is no quality control, there is no economic benefit. In the current world of continually increasing global competition, it is imperative for all manufacturing and service organizations to improve the quality of their products. In today highly competitive scenario, the markets are becoming global and economic conditions are changing fast. Customers are more quality conscious and demand for high quality product at competitive prices with product variety and reduced lead time. It is a data-driven quality strategy used to improve processes. Therefore, this paper aims to review casting defect reduction in manufacturing industry using six sigma.
Leave Your Comment

Related Reviewers

Chat with Expert